Application:
Specially designed for matt
surface transferring
Features:
Easy to release
No corona treatment
Low static, good matt surface
Typical Values:
Properties | Test Method | Unit | Typical Values | |
Thickness | Kinlead | µm | 22 | |
Tickness Variation | ASTM-252-78 | % | ±3.0 | |
Yield | Kinlead | m2/kg | 49.9 | |
Tensile Strength | MD | ASTM D-882 | MPa | 140 |
TD | ASTM D-882 | MPa | 270 | |
Elongation at Break | MD | ASTM D-882 | % | 160 |
TD | ASTM D-882 | % | 55 | |
Friction Coefficient | T/T-US | ASTM D-1894 | 0.35 | |
T/O-US | ASTM D-1894 | 0.60 | ||
Heat Shrinkage | MD | ASTM D-1204 | % | 4.0 |
TD | ASTM D-1204 | % | 2.0 | |
Haze | ASTM D-1003 | % | 38 | |
Gloss | ASTM D-2457 | 16 |